Fast and great quotations, informed advisers to help you choose the correct solution that suits all your requirements, a short creation time, responsible top quality manage and distinct providers for paying and shipping affairs for Fkm Ffkm, Ptfe Sheet, Fep Tube Material, Adhering to the business enterprise philosophy of 'customer first, forge ahead', we sincerely welcome consumers from at your home and abroad to cooperate with us provide you greatest services!
Competitive Price for Materiale Fkm Viton - FKM High Fluorine content (70%) – Huaxia Shenzhou Detail:

Fluoroelastomer FKM Terpolymer Gum-246 series are the terpolymer of vinylidenefluoride,tetrafluoroethylene and hexafluoropropylene.Because of its high fluorine content,its vulcanized rubber has excellent anti oil property and high thermal stability.It also has good mechanical property and can be used in 275℃ for a long time,in 320℃ for a short time.The property of antil oil and anti acid is better than FKM-26,resistance of FKM246 to oil,ozone,radiation,electricity and flamer is similar with FKM26.

Execution standard:Q/0321DYS 005

FKM246-(3)

Quality Specification

Item 246G Test Method/Standards
Density,g/cm³ 1.89±0.02 GB/T533
Mooney Viscosity,ML(1+10)121℃ 50-60 GB/T1232-1
Tensile Strength,MPa≥ 12 GB/T528
Elongation at break,%≥ 180 GB/T528
Compression Set(200℃,70h),%≤ 30 GB/T7759
Fluorine Content,% 70 /
Characteritics and Application Good chemical resistance and liquid resistance /

Note:The above vulcanization systems are bisphenol AF 

Product Use

FKM246 is widely used in aerospace,automotive,machinery,petrochemical,and other fields.For example,the aircraft static/ dynamic seals materials of hydraulic system and lubrication system;used in drilling equipment and oil pipelines;the chemical industry for equipment,flexible pipe connections,liner of pump or corrosion-resistant sealing material,made of pipes to carry solvents or other media,such as corrosion.

Attention

1.Fluoroelastomer terpolymer rubber has good heat stability under 200℃.It will generate trace decomposition if being put at 200-300′C for a long time,and its decomposing speed accelerates at above 320℃,the decomposition products are mainly toxic hydrogen fluoride and fluorocarbon organic compound.When raw fluorous rubber encounters fire,it will release toxic hydrogen fluoride and fluorocarbon organic compound.

2.FKM cannot be mixed with metal powder such as aluminum powder and magnesium powder,or over10% amine compound,if that happens, temperature will arise and several element will react with FKM,which will damage the equipment and operators.

Package, Transportation and Storage

1.FKM is packed in PE plastic bags,and then loaded into cartons,the net weight of each carton is 20kg.

2.FKM is stored in clean,dry and cool warehouse.It is transported according to non-hazardous chemicals,and should keep away from pollution source,sunshine and water during transportation.

FKM246-(3)
FKM26-(4)


Product detail pictures:

Competitive Price for Materiale Fkm Viton - FKM High Fluorine content (70%) – Huaxia Shenzhou detail pictures

Competitive Price for Materiale Fkm Viton - FKM High Fluorine content (70%) – Huaxia Shenzhou detail pictures


Related Product Guide:

Our advancement depends on the superior gear ,superb talents and consistently strengthened technology forces for Competitive Price for Materiale Fkm Viton - FKM High Fluorine content (70%) – Huaxia Shenzhou , The product will supply to all over the world, such as: Brisbane, Hanover, The Swiss, Only for accomplishing the good-quality product to meet customer's demand, all of our products have been strictly inspected before shipment. We always think about the question on the side of the customers, because you win, we win!
  • The customer service staff is very patient and has a positive and progressive attitude to our interest, so that we can have a comprehensive understanding of the product and finally we reached an agreement, thanks!
    5 Stars By Jacqueline from Zambia - 2017.09.26 12:12
    The factory technical staff not only have high level of technology, their English level is also very good, this is a great help to technology communication.
    5 Stars By Amelia from Birmingham - 2018.06.30 17:29
    Leave Your Message